Creep behaviour and life assessment of a cast nickel - base superalloy MAR-M247
HIGH TEMPERATURE MATERIALS AND PROCESSES
Kvapilova, M; Dvorak, J; Kral, P; Hrbacek, K; Sklenicka, V, 2019: Creep behaviour and life assessment of a cast nickel - base superalloy MAR-M247. HIGH TEMPERATURE MATERIALS AND PROCESSES 38, p. 590 - 600, doi: 10.1515/htmp-2019-0006