Influence of Al-Si diffusion coating on low cycle fatigue properties of cast superalloy Inconel 738LC at 800 degrees C

ADVANCES IN FRACTURE AND DAMAGE MECHANICS X

Julis, M; Obrtlik, K; Pospisilova, S; Podrabsky, T; Polak, J, 2012: Influence of Al-Si diffusion coating on low cycle fatigue properties of cast superalloy Inconel 738LC at 800 degrees C. ADVANCES IN FRACTURE AND DAMAGE MECHANICS X 488-489(1), p. 307 - 310, doi: 10.4028/www.scientific.net/KEM.488-489.307