Misfit in Inconel-Type Superalloy

ADVANCES IN MATERIALS SCIENCE AND ENGINEERING

Strunz, P; Petrenec, M; Davydov, V; Polak, J; Beran, P, 2013: Misfit in Inconel-Type Superalloy. ADVANCES IN MATERIALS SCIENCE AND ENGINEERING , doi: 10.1155/2013/408347