Modeling load-displacement curve and pop-in effect in nanoindentation tests

20TH EUROPEAN CONFERENCE ON FRACTURE

Sandera, P; Pokluda, J; Schoberl, T; Hornikova, J; Cerny, M, 2014: Modeling load-displacement curve and pop-in effect in nanoindentation tests. 20TH EUROPEAN CONFERENCE ON FRACTURE 3, p. 1111 - 1116, doi: 10.1016/j.mspro.2014.06.181