Stage I fatigue cracking in MAR-M 247 superalloy at elevated temperatures

21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21)

Smid, M; Hutar, P; Hornik, V; Hrbacek, K; Kunz, L, 2016: Stage I fatigue cracking in MAR-M 247 superalloy at elevated temperatures. 21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21) 2, p. 3018 - 3025, doi: 10.1016/j.prostr.2016.06.378