Molybdenum diselenide thin films grown by atomic layer deposition: An XPS analysis

SURFACE SCIENCE SPECTRA

RODRIGUEZ PEREIRA, J.; ZAZPE, R.; CHARVOT, J.; BUREŠ, F.; MACÁK, J., 2020: Molybdenum diselenide thin films grown by atomic layer deposition: An XPS analysis. SURFACE SCIENCE SPECTRA 27(2), p. 024006-1 - 8, doi: 10.1116/6.0000354; FULL TEXT