Comparative Study of Microstructure and High Temperature Low Cycle Fatigue Behaviour of Nickel Base Superalloys Inconel 713LC and MAR-M247

KEY ENGINEERING MATERIALS (WEB)

ŠULÁK, I.; OBRTLÍK, K.; ČELKO, L., 2016: Comparative Study of Microstructure and High Temperature Low Cycle Fatigue Behaviour of Nickel Base Superalloys Inconel 713LC and MAR-M247 . KEY ENGINEERING MATERIALS (WEB) , p. 86 - 3, doi: 10.4028/www.scientific.net/KEM.713.86; FULL TEXT