STUDY OF SURFACE RELIEF EVOLUTION IN CYCLICALLY STRAINED SUPERALLOY IN738LC USING ADVANCED EXPERIMENTAL TECHNIQUES
CHEMICKE LISTY
Julis, M; Kusmic, D; Pospisilova, S; Prusa, S; Obrtlik, K; Dluhos, J; Podrabsky, T, 2011: STUDY OF SURFACE RELIEF EVOLUTION IN CYCLICALLY STRAINED SUPERALLOY IN738LC USING ADVANCED EXPERIMENTAL TECHNIQUES. CHEMICKE LISTY 105, p. S814 - S815