Use of powder liquid method of aluminide diffusion coatings formation on inconel 713 LC nickel-based superalloy
Materials and Manufacturing Processes
CELKO, L., KLAKURKOVA, L., MAN, O., SVEJCAR, J., 2009: . MATERIALS AND MANUFACTURING PROCESSES 24(10-11), p. 1155 - 1161